Silicone rubber for plaster /gypsum moulding (Tin catalyst series)

Home / Chemicals / Catalysts / Silicone rubber for plaster /gypsum moulding (Tin catalyst series)
Custom Search
Detailed Silicone rubber for plaster /gypsum moulding (Tin catalyst series) Description:


Specifications

Silicone rubber Features:1) Low linear shrinkage 2)Good operation 3) high tear strength 4)curing agent for free 5)Easy de-mold

Sell Silicone rubber for plaster /gypsum moulding (Tin catalyst series)

Silicone rubber HY-638 application:
Silicone RTV (HY-638 ) is two parts condensation liquid silicone rubber that can be cure under room temperature. silicone rubber mainly used for the manufacturer of products made of unsaturated resin, epoxy resin, polyurethane, etc.


Silicone rubber(HY-638) features:
HY-638# silicone rubber is mainly with the advantages of good tensile strength, high tear strength, high temperature resistance, high duplication times and repeated use, etc.

Silicone rubber(HY-638) is the most suitable for small products or fine and precision products which is difficult to demould. This silicone rubber is one of the products with the highest use level in the production of craftwork gifts and the shrinkage less than 0.2%.

Silicone rubber(HY-638) datasheet :
Model
Appearance
Viscosity (cs)
Hardness (Ao)
Tensile Strength (kgf/c)
Tear Strength (kgf/)
Elongation (%)
Mixing ratio(%)
Operating Time(H)
Curing Time(H)
638
White
14000~16000
25~28
≥35
≥25
≥500
2~3
0.5
2~4

Silicone rubber (HY-638 RTV-2) instruction:
1. Adding curing agent 1%, the silicone can still be operated within 2.5 hours and can be
demoulded after 6-8 hours.
2. Adding curing agent 2%, the silicone can still be operated within 50 minutes to 1 hour and
can be demoulded after 2-3 hours.
3. Adding curing agent 3%, the silicone can still be operated within 28 - 30 minutes and can
be demoulded after 1.5-2 hours.
4. Adding curing agent 4%, the silicone can still be operated within 10 - 15 minutes and can
be demoulded after 1 -1.5 hours.

Frequently asked questions of moulding silicone rubber
Why does the silicone rubber mold have few molding times?

The silicone rubber mold has few molding times is due to follwoing reasons: adding too much silicone oil which will destroy the molecular of silicone rubber; making the mold for small and fine detailed products with higher hardness silicone rubber which is easy to break; making the mold for large products with soft silicone rubber which will reduce the tensile and tear strength of the mold, and the mold will have deformation. Thus, we should take the proper silicone rubber to make the mold for suitable products.

Silicone rubber for plaster /gypsum moulding (Tin catalyst series)
  • Model: Silicone rubber 638# 788#
  • Packing: 20kg/pail 25kg/pail 200kg/pail
  • Terms of Payment: L/C,T/T,Western Union
  • Delivery Time: 3days
  • Products ID: 144466
  • Product Category: Catalysts
  • Post date: May 23, 2014
Our company is specialized exporter, manufacturer and supplier of Silicone rubber for plaster /gypsum moulding (Tin catalyst series) in China .


           

Manufacturer/supplier's information

Company: Dongguan Tinpak Co., Ltd.
Address: Tinpak Bldg., Tongyue Road, Tongsha Industrial District, Dongguan City, China 523128
Region: Dongguan, Guangdong, China
Contact Person: Daisy Huang
Telephone: 086-769-23171505

Other Products From This Company


Food Grade Injection Silicone Rubber Products
Specifications 1.Very low shrinkage 2.Special produce accordingly to your request 3.Easy removal fo complex ...

Silicone Rubber for human body decoration Mould Making
Specifications Human boby silicone rubber is a kind elastic silicon rubber mold which features with resistance to ...

RTV-2 Mould Making Silicone Rubber for soap molds
Specifications Silicon features:1) For soaps mold making.2) high tensile, tear-strength.etc.3) low shrinkage 4) ...

RTV silicone rubber for manual molding
Specifications Silicon features: 1) For mold making, for pad printing. 2) high tensile, tear-strength.etc.3) low ...