Detailed Modified Coal Tar Pitch Description:
Softening point(Ball and ring method)℃ 100~115 100~120 ; TI Content(Extraction method),% 28~34 >26 ; QI Content,% 8~14 6~15 ; Resin content,% No less than 18 16 ; Agglomerating value,% No less than 54 50 ; Ash,% No more than 0.3 0.3 ; Water,% No more than 5 5