Detailed Refractory Brick for Glass Smelting Furnace Description:
1) Zirconia-mullite brick for glass smelting furnace: a) Al2O3 (%): 60 ; b) Fe2O3 (%): 0.5 ; c) ZrO (%): 20 ; d) Porosity (%): 20 ; e) Bulk density (g/cm³): 3.05 ; f) Cold crushing strength (MPa): 80 ; g) Refractoriness under load 0.2MPa KD (oC): 1,650. 2) Burned brick based on fused mullite: a) Al2O3 (%): 75 ; b) Fe2O3 (%): 0.3 ; c) SiO2 (%): 24 ; d) Porosity (%): 17 ; e) Bulk density (g/cm³): 2.7 ; f) Cold crushing strength (MPa): 90 ; g) Refractoriness under load 0.2MPa KD (oC): 1,700 ; h) Permanent change 1,500oC x 3hrs. (%): ±0.1
- Products ID: 23665
- Product Category: Refractory
- Post date: Aug 15, 2008
Our company is specialized exporter, manufacturer and supplier of Refractory Brick for Glass Smelting Furnace in china.